Technology Sharing
2024.02.20
Case Analysis | Common Failure Causes Analysis of Photovoltaic Module Backboard
The photovoltaic module back panel, as the outermost material of the protective module, directly withstands the influence of external environmental climate and repeated stress. The adhesive performance, UV resistance, and mechanical strength of the backboard material are key factors affecting the service life of the entire component.
Detail
2024.02.05
Case Study | Cracking failure analysis and composition analysis of electronic product fixtures
If the fixture of an electronic product cracks in the screw column, the defective results will still be reproduced by adjusting the screw size, torque setting and assembly process parameters in the early stage. It is understood that the failure parts come from multiple production batches, but the raw materials are concentrated in the same batch, considering that the failure mode may be the failure of the formula process, so the quantitative analysis of the whole composition and failure analysis
Detail
2024.01.23
Comparison Case | Laboratory Comparison Summary and Analysis of Plastic Tensile Properties in 2023, Attached with Comparison Plan for 2024
In order to test the testing ability of various laboratories to determine the tensile properties of plastics, the National High tech Materials Analysis and Testing Center organized a laboratory comparison activity for this project in 2023, which verified the accuracy of the measurement results.
Detail
2024.01.16
Product recommendation | Quality control samples for plastic density testing
Quality control samples for plastic density testing are prepared by National High Polymer Materials Industry Innovation Center Co., Ltd. They are mainly used for calibration of polymer material density measurement instruments, confirmation and evaluation of analysis and measurement methods, and quality control of analysis and measurement processes.
Detail
2024.01.02
Selection of temperature and nominal load parameters for plastic melt finger testing
The confirmation and adjustment of processes in production processes such as injection molding have a certain effect. If the melt index is too large, it indicates that the product performance of the raw material after processing is poor, making it easy to process and shape, but cracking and other situations may occur;
Detail
2023.11.15
The key role and advantages of vibration testing in evaluating the durability performance of automotive components
The vibration test bench can simulate the dynamic response of vehicles under road excitation, and conduct a series of controllable vibration simulations in the laboratory to test whether automotive components can withstand the impact of vibration environment during transportation, assembly, and use during their lifecycle. This can help detect electrical short circuits, loose fasteners, seal failures, and cracks as soon as possible.
Detail
2023.10.10
Research on the Effect of Frequency on Rubber Viscoelasticity in DMA Stretching Mode
This article selects frequency as the sole variable to study the viscoelastic changes of rubber. The aim is to summarize the effect of different frequencies on the testing of rubber viscoelasticity using thin film stretching fixtures in DMA by comparing test results.
Detail
2023.09.19
What is Material Card MAT24 in Mechanical Simulation? How to accurately obtain it?
MAT24 is a commonly used elastic-plastic material model that can define the strain rate effect of materials through stress-strain curves or functions of strain rate effects.
Detail
2023.09.01
The influence of sample and method differences on the CLTE testing of polypropylene TMA
Static Thermomechanical Analysis (TMA) refers to the technique of measuring the relationship between deformation and temperature of a substance under non vibration loads under programmed temperature control.
Detail
2023.08.22
Study on Thermogravimetric Analysis for Testing Low Content Carbon Black in Fiberglass Reinforced PP and Modified PA6 Plastics
At present, the testing methods for carbon black content are mainly divided into two categories: TGA method and direct combustion method, among which using a carbon black tester for testing is a typical direct combustion method.
Detail
2023.08.08
Analysis and improvement of the causes of bending and whitening of PP composite materials
Among automotive materials, polypropylene (PP) has advantages such as excellent chemical corrosion resistance, high stiffness, low density, and low cost, and is widely used in exterior and interior parts of automobiles.
Detail
2023.07.13
Plastic creep - not just a simple description of deformation
Why do some plastic products suddenly break or deform after long-term use?