Functional membrane materials
Rubber and elastomers
Biodegradable plastics

In order to meet people's needs for safety, environmental protection and green production, we focusing on key areas such as automobiles, rail transit, electronic information, new energy, energy saving and environmental protection. we work on developing high-performance resins, special rubbers and elastomers, high-performance fibers and their composites, functional membrane materials, electronic chemicals, water-based coatings and other green petrochemicals. We have served many petrochemical enterprises, helped them breaking through the supply bottleneck of key raw materials in the upstream, speeded up the industrialization and application of blank varieties in China, and promoted Chinese petrochemical industry to higher end of the global value chain.


Functional membrane materials

Functional membrane materials refer to membrane materials with one or more functions such as optics, electrics, separation and barrier, which are widely used in consumer electronics, screen display components, FPC manufacturing, new energy batteries, automotive electronics and many other fields.


Functional membrane materials
  厚度   GB/T 6672-2001、ASTM D374-19、ISO 4593:2014
  拉伸性能   GB/T 1040.1-2006、GB/T 13022-91、ASTM D882-18、ISO 527-1:2019
  剥离强度   GB/T 2792-2014
  水分含量   GB/T  26793-2011
  热收缩率   ASTM D2732、GB/T3519
  摩擦系数   GB/T 10006-88
  表面张力   GB/T 14216-2008、ASTM D2578-19、ISO 8296:2018
  透明度   GB/T 2410-2008、ASTM D1746-15、ISO 14782:2006
  气体渗透率   GB/T 1038-2000、ASTM D1434-2019、ISO 15105-1:2019
  透气性   GB/T 1038-70
  孔隙率   GB/T 36363-2018、ASTM D2873
  穿刺强度   ASTM F1306、ISO 7765-1
  电性能   GB/T 13542.2-2009


Rubber and elastomers
Rubber and elastomer materials
  未硫化橡胶门尼粘度   GB/T 1232.1-2000、GB/T 1233-1992、ISO 289-1:2005、ISO 289-2-1994、ASTM D1646-2004、JIS K6300-1:2001
  硬度   GB/T 531-2008、GB/T6031-2017、ASTM D1415-2004、ASTM D2240-2015、ISO 7619-1:2010
  拉伸性能   GB/T 528-2009、ASTM D412-2016、ISO 37:2017、JIS K6251:1993、DIN 53504-1994
  撕裂性能   GB/T 529-2008、ASTM D624-2016、ISO 34-1:2015、JIS K6252:2001
  压缩永久变形   GB/T 7759-1996、ASTM D395-2020、ISO 815-1:2014、JIS K6262:1997
  剥离强度   GB/T 2791-1995、ASTM D413-2018、ISO 36:2019
  回弹性   GB/T 1681-1991、ASTM D2632-2013、ISO 4662:2015、JIS K6255:1996、DIN 53512-2000
  耐磨性   GB/T 9867-2008、ASTM D5963-2017、ISO 4649:2010
  磨耗性   GB/T1689-1998、GB/T9867-1988、ASTM D5963-2004
  低温脆化   GB/T 1682-1994、GB/T15256-1994、GB/T 7758-2002、ASTM D2137-2017、ASTMD1329-2002、ASTM D746-2004、ISO 812:2004、ISO 2921:2005
  电性能   GB/T 1692-1992、GB/T 1693-1989、GB/T1694-1989、GB/T 1695-2005、GB/T2439-2001
  耐化学品   GB/T 1690-2005、ASTM D471-2016、ISO 1817:2015
  耐油测试   GB/T 1691-2008、ASTM D471-2016、ISO 1817:2015
  燃烧性能   GB/T 10707-89、GB/T 13488-92、UL94-1996
  热空气老化性能   GB/T 3512-2001、ISO188-1998、ASTM D573-2004、DIN53508-2000、JIS K 6257-2003
  耐臭氧老化性能   GB/T 7762-2003、GB/T 13642-1992、ASTM D518-1999、ASTMD1149-1999、ASTM D1171-1999、ASTM D3395-1999、DIN 53509-1-2001、JIS K6259-2004



Rubber and elastomer products
  减震器类   HG 2864-1997   车辆用橡胶缓撞器
  HG/T 3080-2009   防震橡胶制品用橡胶材料
  HG/T 2866-2003   橡胶护舷
  JT/T 4-2004   公路桥梁板式橡胶支座
  JT 391-2009   公路桥梁盆式橡胶支座
  TB/T 1893-2006   铁路桥梁板式橡胶支座
  TB/T 2331-2004   铁路桥梁盆式橡胶支座
  JG 118-2000   建筑隔震橡胶支座
  HG/T 2289-2001   可曲挠橡胶接头
  JT/T 327-2004   公路桥梁伸缩装置
  HG/T 3328-2006   铁路混凝土枕轨下用橡胶垫板
  JT/T 529-2004   预应力混凝土桥梁用塑料波纹管
  GB/T 17955-2009   桥梁球型支座
  GB 20688.4-2007   橡胶支座第4部分普通橡胶支座
  HG/T 2287-2008   印刷胶辊
  HG/T 2447-2003   胶辊 第4部分印染胶辊
  HG/T 2446-2005   胶辊 第5部分造纸胶辊
  HG/T 2445-2005   胶辊 第6部分电子打字(印)机胶辊
  HG/T 2697-2001   胶辊 第二部分 聚氨酯胶辊
  HT/T 2013-2001   胶辊 第三部分 织物预缩橡胶毯
  HG/T 2196-2004   汽车用橡胶材料分类系统
  GB/T 12730-2008   一般传动用窄V带
  HG/T 2578-1994   汽车液压制动缸用橡胶护罩
  HG/T 2491-2009   汽车用输水橡胶软管和纯胶管
  HG/T 3088-1999   车辆门窗橡胶密封条
  GB/T 15846-2006   集装箱门框密封条
  HG/T 2810-2008   往复运动橡胶密封圈材料
  胶辊类   HG/T 2811-1996   旋转轴唇形密封圈橡胶材料
  GB/T 9877-2008   液压传动旋转轴唇形密封圈设计规范
  GB/T 15326-1994   旋转轴唇形密封圈外观质量
  GB/T 13871.1-2007   密封元件为弹性体材料的旋转轴唇形密封圈第1部分:基本尺寸和公差
  HG/T 2021-1991   耐高温滑油0型橡胶密封圈材料
  GB/T 3452.2-2007   液压气动用0形橡胶密封圈
  HG/T 3089-2001   燃油用0形橡胶密封圈材料
  HG/T 2181-2009   耐酸碱橡胶密封件材料
  HG/T 2579-2008   普通液压系统用0形橡胶密封圈材料
  GB/T 3452.1-2005   液压气动用0形橡胶密封圈
  GB/T 3452.2-2007   液压气动用0形橡胶密封圈
  汽车类   GB/T 12002-1989   塑料门窗用密封条
  HG/T 3099-2004   建筑橡胶密封垫预成型实心硫化的结构密封垫用材料规范
  TB/T 1964-1987   客车门窗用密封条
  JB/T 7757.2-2006   机械密封用0形橡胶圈
  JC/T 946-2005   混凝土和钢筋混凝土排水管用橡胶密封圈
  JC/T 483-2006   聚硫建筑密封胶
  HG/T 3326-2007   采煤综合机械化设备橡胶密封件用胶料
  JC/T 748-1996   预应力与自应力钢筋混凝土管用橡胶密封圈
  GJB 250A-1996   耐液压油和燃油丁腈橡胶胶料规范
  GB/T 15325-1994   往复运动橡胶密封圈外观质量
  GB/T 10708.1-2000   往复运动橡胶密封圈结构尺寸系列第一部分
  密封制品材料   GB/T 10708.2-2000   往复运动橡胶密封圈结构尺寸系列第二部分
  GB/T 10708.3-2000   往复运动橡胶密封圈结构尺寸第三部分
  GB 5135.11-2006   自动喷水灭火系统
  JC/T 976-2005   道桥嵌缝用密封胶
  GB/T 21873-2008   橡胶密封件给、排水管及污水管道用接口密封圈材料规范
  HG 2865-1997   汽车液压制动橡胶皮碗
  HG 2950-1999   汽车制动气室橡胶隔膜
  GJB 5258-2003   航空橡胶零件及型材用胶料规范
  GB/T 10716-2000   同步带拉伸性能试验方法
  GB 10717-1989   同步带齿剪切强度试验方法
  GB/T 7762-2003   硫化橡胶或热塑性橡胶耐臭氧龟裂静态拉伸试验
  GB/T 1682-1994   硫化橡胶低温脆性的测定单试样法
  GB/T 3512-2001   硫化橡胶或热塑性橡胶热空气加速老化和耐热试验
  GB/T 11545-2008   带传动汽车工业用V带疲劳试验
  GB/T 3686-1998   三角带全截面拉伸性能试验方法
  GB 12732-2008   汽车V带
  GB/T 7762-2003   硫化橡胶或热塑性橡胶耐臭氧龟裂静态拉伸试验
  GB 16897-1997   制动软管


Biodegradable plastics

Biodegradable plastics are polymer materials with excellent performance, which can be completely decomposed by environmental microorganisms after being discarded, and ultimately become an integral part of the carbon cycle in nature by being inorganic.


 "Paper" is a typical biodegradable material, while "synthetic plastic" is a typical polymer material. Therefore, biodegradable plastics are polymer materials that combine the properties of both paper and synthetic plastics.


General requirements
  绿色产品评价塑料制品   2017343-T-469
  环境标志产品技术要求一次性餐饮具   HJ/T 202-2005
  环境标志产品技术要求 包装制品   HU/T 209-2005
  降解塑料的定义、分类、标识和降解性能要求   GB/T 20197-2006
  淀粉基塑料   QB/T 4012-2010
  可堆肥塑料技术要求   GB/T 28206-2011
  包装与包装废弃物 第7部分:生物降解和堆肥   GB/T 16716.7-2012
  生态设计产品评价规范第2部分;可降解型料   GB/T32163.2-2015
  生物基材料定义、术语和标识   20171127-T-469


Product standards
  快递   快递封装用品  第1部分:封套   GB/T 16606.1
  邮政业封装用胶带第2部分:生物降解胶带   YZ/T 0160.2-2017
  《邮政业包装填充物技术要求》   YZ/T 0116-2018
  快件航空运输信息交换规范   GB/T 38726-2020
  全生物降解物流快递运输与投递用包装塑料膜、袋   GB/T 38727-2020
  膜袋   生物分解塑料垃圾袋   GB/T 28018-2011
  生物聚酯连卷袋   GB/T 33798-2017
  淀粉基型料购物袋   GB/T 38079-2019
  生物降解塑料购物袋   GB/T 38082-2019
  吹塑薄膜用改性聚酯类生物降解塑料   GB/T 29646-2013
  全生物降解农用地面覆盖薄膜   GB/T 35795-2017
  生物制造聚羟基烷酸酯(PHA)吹塑薄膜   GB/T 30293-2013
  餐饮具   一次性可降解餐饮具降解性能试验方法   GB/T 18006.2-1999
  纸浆模型餐具   GB/T 36787-2018
  全生物降解饮用吸管   20192206-T-469
  酒店客房用易耗塑料制品   GB/T 24453-2009
  植物纤维模塑制品通用技术要求   GB/T 30406-2013
  聚3-羟基丁酸-戊酸酯/聚乳酸(PHBV/PLA)共混物长丝   GB/T 34239-2017
  秸秆纤维基聚丙端改性料   GB/T 36941-2018
  熔融沉积成型用聚乳酸(PLA)线材   GB/T 37643-2019
  聚乳酸/聚丁二酸丁二醇酯复合材料空气过滤板   GB/T 37836-2019
  聚乳酸热成型一次性验尿杯   GB/T 37857-2019


塑料薄膜及塑料包装材料主要性能测试
  强度&断裂伸长率   GB/T1040.1&1040.3、ISO 527-1&3、ASTM D882 
  撕裂强度   QB/T113、GB/T16578.1、ASTM D1004、ISO6383、ASTM D1938 
  摆锤冲击   GB/T16578、ASTM D1922、ISO6383-2 
  老化测试 ( 仅针对光降解塑料)   GB/T 16422.2、ISO 4892-2
  薄膜抗冲击   GB/T 9639.1、ASTM D1709、EN ISO 7765-1
  穿刺强度测试   GB/T 10004、GB/T 21302、ASTM D5748、EN 14477、ASTM F1306
  透光率   GB/T2410、ASTM D1003、ISO13468-1、ASTM E903
  透水蒸气测试   GB/T1037、GB/T16928、ISO2528、ASTM D1653、ISO15106-2
  氧气透过率   GB/T1038、ASTM D1434、ISO2556、JIS K7126-1
  热合强度   QB/T2358、ASTM F88/F88M


Resin standard
  聚乙烯醇树脂命名   GB/T12010.1-1989
  可生物降解淀粉树脂   GB/T 27868-2011
  聚乳酸   GB/T 29284-2012
  聚丁二酸丁二酯PBS   GB/T 30294-2013
  植物纤维模塑制品通用技术要求   GB/T 30406-2013
  生物制造聚羟基烷酸酯PHA   GB/T 30293-2013
  聚碳酸亚丙酯PPC   GB/T 31124-2014
  生物降解聚对苯二甲酸-己二酸丁二酯(PBAT)   GB/T 32366-2015
  聚丁二酸-己二酸丁二酯(PBSA)树脂   GB/T 34255-2017
  热塑性淀粉通用技术要求   GB/T 33796-2017
  秸秆纤维基聚丙烯改性料   GB/T 36941-2018
  聚己内酯(PCL)   GB/T 37642-2019


Degradation degree detection method
  材料在特定微生物作用下潜在生物分解和崩解能力的评价   GB/T 19275-2003
  水性培养液中材料最需氧生物分解能力的测定采用测定密闭呼吸计中需氧
量的方法
  GB/T 19276.1-2003
  水性培养液中材料最终需氧生物分解能力的测定采用测定释放的二氧化碳
的方法
  GB/T 19276.2-2003
  在定义堆肥化中试条件下塑料材料崩解程度的测定   GB/T 19811-2005
  在定义堆肥化中试条件下塑料材料崩解程度的测定   GB/T 19811-2005
  土壤中塑料材料最终需氧生物分解能力的测定 采用测定密闭呼吸计中需氧
量或测定释放的二氧化碳的方法
  GB/T 22047-2008
  受控堆肥条件下材料最终需氧生物分解能力的测定 采用测定释放的二氧化
碳的方法第1部分:通用方法
  GB/T 19277.1-2011
  受控堆肥条件下材料最终需氧生物分解能力的测定 采用测定释放的二氧化
碳的方法第2部分:用重量分析法测定实验室条件下二氧化碳的释放量
  GB/T 19277.2-2013
  塑料在高固体份堆肥条件下最终厌氧失物会解能力的要定翠用分析测定释
放生物气体的方法
  GB/T 33797-2017