2026.01.27
Characterization Methods for Micromechanical Behavior of Composites: Nanoindenter + AFM + Polarizing Microscope
PEEK/CF composites exhibit excellent performance, but their complex multiphase microstructure has a decisive impact on their properties. Around the fibers, a highly oriented transcrystalline layer is often formed due to heterogeneous nucleation. In addition, spherulites and amorphous regions are also present in the matrix. The local modulus, hardness of these different morphological regions, and their responses under load directly affect the overall stiffness, strength, toughness, and damage evolution behavior of the composites.
Detail
2026.01.20
New Energy Vehicles (NEV),MAT_58 Material Card,Composite Material Undertrays
Application of MAT_58 Material Card in Simulation Analysis of Composite Material Undertrays for New Energy Vehicles
Detail
2026.01.20
Notice | 2026 Laboratory Comparison Plan
As an important quality control activity, laboratory comparison is of great significance for improving laboratory management level, the operational skills of testing personnel, and ensuring the accuracy and validity of test results. It is not only an effective supplement to the internal quality control of laboratories, but also an important means to enhance customers' trust in laboratories and improve their competitiveness. To further promote technical exchanges and development in the field of polymer material testing, National Advanced Materials Analysis and Testing Center will continue to carry out 17 laboratory comparison activities in 2026. The relevant arrangements are hereby notified as follows:
Detail
2026.01.10
Live Preview | Core Interpretation of JIS D0205 Standard for Automotive Interior Parts Photoaging Test
From history to standards, from principles to applications: fully understanding the core role and testing logic of sunshine carbon arc lamps in JIS D0205.
Detail
2026.01.13
3D Profile Scanner: The "Sharp Eye" for Component Simulation Model Comparison and Warpage Analysis
In modern manufacturing, especially in high-end equipment, automotive industry, precision electronics and new materials, the surface and three-dimensional morphology of products are no longer simple “appearance” issues, but core quality indicators directly related to performance, reliability and service life.A micron-level step, a nanometer-scale scratch, or an inconspicuous warpage deformation can all become the “Achilles’ heel” of product failure.Traditional contact measurement and two-dimensional visual inspection are often inadequate when facing complex curved surfaces, special-shaped structures and micro-morphologies, with incomplete data and low efficiency.
Detail
2026.01.13
Accurate Evaluation of Cathode Material Thermal Stability Using DSC/TGA to Secure the Safety of Power Batteries
High-nickel cathode materials are currently the mainstream high-specific-energy cathode materials, featuring high capacity, appropriate cost, and other advantages. However, the thermal stability of high-nickel cathode materials still needs to be improved, which largely limits their upper application limit, especially in fields such as electric vehicles and large-scale energy storage. At present, the evaluation mechanism for the thermal stability of high-nickel cathode materials is not yet clear, and there is a lack of uniform standards for its measurement. Therefore, it is crucial to develop a unified and standardized thermal stability evaluation mechanism.
Detail
2026.01.06
Gel Content Determination Method for Characterizing Crosslink Density of Crosslinked Polyethylene (XLPE) Used in Cables
Owing to its unique electrical insulation properties, crosslinked polyethylene (XLPE) can effectively prevent current leakage and arc formation. Currently, one of its largest application areas is in wires and cables. This characteristic is closely related to the crosslinking degree of XLPE. Crosslinking of polyethylene increases the barrier paths for current passage, thereby improving insulation resistance; the higher the crosslinking degree, the greater the insulation resistance. However, excessive crosslinking will lead to insufficient elasticity and susceptibility to aging, thus affecting service life. Therefore, an appropriate crosslinking degree of polyethylene must be maintained in the production process to meet application requirements.
Detail
2026.01.06
Plastic Spiral Flow Test: The Core Method for Evaluating Material Mold Filling Capability
In plastic injection molding, ensuring the melt can completely fill the mold cavity is the first step to successful production. As a standardized and intuitive evaluation method, the Spiral Flow Test is widely used to quantify the flowability of resins, thereby directly predicting their mold-filling capability. By measuring the flow length of the resin in a spiral flow channel under specific processing conditions, this method provides critical data for material selection, process setting, and quality control.
Detail
2025.12.23
Two New SVHC Substances Added by the EU: How to Achieve Rapid Detection via GC-MS?
On December 15, 2025, the European Chemicals Agency (ECHA) reached a unanimous agreement at its December meeting to identify n-hexane as a Substance of Very High Concern (SVHC). Another substance, 4,4'-[2,2,2-trifluoro-1-(trifluoromethyl)ethylidene]diphenol (BPAF) and its salts, was designated as an SVHC without the involvement of the Committee. ECHA will add these two substances to the Candidate List of Substances of Very High Concern in February 2026, bringing the total number of substances on the list to 253 at that time.
Detail
2025.12.23
Multi-scale Fluid Characterization: Decoding the Deformation Language of Materials from "Solid State" to "Liquid State" via Rotational Rheometers
A rotational rheometer is a core instrument for studying the rheological behaviors of materials (such as viscosity, elasticity, and yield stress), and it is widely used in fields including polymers, food, cosmetics, pharmaceuticals, inks, and coatings. It applies controllable stress or strain to samples via rotating fixtures, measures the mechanical responses of the materials, and thereby analyzes their flow and deformation characteristics.
Detail
2025.12.16
Optimization Scheme for Shear Strength Testing of Aerospace-grade Adhesives Based on ASTM D5656
The foundation and objective of modern aircraft design lie in achieving low structural weight, high strength and high efficiency. These characteristics are attained through the utilization of advanced materials (such as high-strength aluminum alloys and carbon fiber-reinforced composite materials) as well as the development of special structural solutions. One such solution is to replace mechanical fasteners (e.g., fasteners, rivets, etc.) with bonded joints. The primary advantage of bonded joints is their lower weight compared to mechanical fasteners. However, the adoption of bonded joints also introduces new challenges, whether in manufacturing, testing or aircraft structural modeling. Accurate measurement of the mechanical properties of adhesives, especially the shear modulus, is crucial for the efficient design of aircraft structures.
Detail
2025.12.16
Sharing of Test Method for Compression of Composite Materials per ASTM D6641
Benefiting from their outstanding specific strength, specific stiffness and designability, composite materials have been widely applied in high-end equipment fields such as aerospace, rail transit and automotive industry. Among various mechanical properties, compressive performance is a key indicator for evaluating the load-bearing capacity of composite structures. However, due to their characteristics including anisotropy and relatively low interlaminar strength, the accurate measurement of compressive performance has long been a key challenge and research priority in the field of material testing.
Detail